Propiedades materiales Norm Symbol/Unit F F plus T
Densidad DIN EN 623-2 ρ [g/cm3] >3.10 >3.16 >3.21
Porosity DIN EN 623-2 P [%] <3.0 <1.0 <1.0
Mean grain size   [μm] <5 <5 <2
Grain size distribution   [μm]      
Phase composition     α-SiC α-SiC α-SiC,
YAG
Vickers hardness DIN EN 843-4 HV 1 [GPa] 25.5 25.5 22.5
Knoop hardness DIN EN 843-4 HK 0.1 [GPa] 24.5 24.5 21.0
Young's modulus DIN EN 843-2 E [GPa] 410 420 420
Weibull modulus DIN EN 843-5 m 10 15 15
Flexural strength,
4-pt bending
DIN EN 843-1 σB [MPa] 400 510 550
Compressive strength   σD [MPa] 2200 2200 2500
Poisson ratio   ν 0.17 0.17 0.16
Fracture toughness
(SENB)
  Klc [MPa·m0,5] 4 4 6
Coefficient of
thermal expansion
DIN EN 821-1        
20°C - 500°C   α [10-6/K] 4.1 4.1 3.5
500°C - 1000°C   α [10-6/K] 5.2 5.2 5.2
Specific heat at 20°C DIN EN 821-3 cp [J/g K] 0.6 0.6 0.6
Thermal conductivity
at 20°C
DIN EN 821-2 λ [W/mK] 125 125 75
Thermal stress
parameters
calculated        
R1 = σB·(1-ν) / (α·E)   R1 [K] 198 246 314
R2 = R1·λ   R2 [W/mm] 25 31 24
Specific electrical
resistance at 20°C
DIN EN 50359 ρ [Ω cm] 106-108 106-108 102-103
  Silicon Carbide
Material properties Norm Symbol/Unit C P G
Density DIN EN 623-2 ρ [g/cm3] >3.10 >2.76-
2.89
>3.02
Porosity DIN EN 623-2 P [%] <3.0 10-14 <3.0
Mean grain size   [μm] bimodal <5 bimodal
Grain size distribution   [μm] 10-1500   10-1000
Phase composition     α-SiC α-SiC α-SiC,
graphite
Vickers hardness DIN EN 843-4 HV 1 [GPa] 25.5 23.5 24.5
Knoop hardness DIN EN 843-4 HK 0.1 [GPa] 24.5 21.6 23.0
Young's modulus DIN EN 843-2 E [GPa] 410 340 390
Weibull modulus DIN EN 843-5 m 10 15 14
Fuerza flexible,
Flexión de 4 puntos
DIN EN 843-1 σB [MPa] 400 225 230
Compressive strength   σD [MPa] 2500 2000 2500
Poisson ratio   ν 0.17 0.17 0.16
Fracture toughness
(SENB)
  Klc [MPa·m0,5] 3.5 3 3
Coeficiente de
expansión térmica
DIN EN 821-1        
20°C - 500°C   α [10-6/K] 4.1 3.5 4.0
500°C - 1000°C   α [10-6/K] 5.2 5.6 5.0
Specific heat at 20°C DIN EN 821-3 cp [J/g K] 0.6 0.6 0.6

Más información>>

1.Carburo de tungsteno
2.Bolas de carburo de tungsteno
3.Rebabas de carburo de tungsteno
4.Insertos de carburo de tungsteno
5.Placas de carburo de tungsteno


CHINATUNGSTEN ONLINE se ha especializado en la fabricación de productos de tungsteno, especialmente productos de carburo cementado durante más de 20 años. Si tiene alguna consulta sobre los productos en este sitio web, no dude en enviarnos un correo electrónico por: sales@chinatungsten.com

Address: 3F, No.25 WH Rd., Xiamen Software Park Ⅱ, FJ 361008,China
Phone:+86-592-5129696,+86-592-5129595;Fax:+86-592-5129797;Email:sales@chinatungsten.com
Certified by MIIT:闽B2-20090025 闽ICP备05002525号-1
Copyright©1997 - ChinaTungsten Online All Rights Reserved